GH2132 nickel based superalloy with excellent mechanical properties

 GH2132 is a nickel-based superalloy with excellent mechanical properties. After solution treatment, the strength, hardness and toughness of GH2132 will be improved.

The tensile strength of GH2132 after solution is usually between 700 MPa and 900 MPa. The dissolved GH2132 alloy has a high tensile strength, which enables it to withstand large tensile forces without plastic deformation or fracture. This makes GH2132 alloy have good mechanical properties under high temperature, high pressure and corrosive environment. For GH2132, the solution treatment temperature is generally between 1150 ° C and 1200 ° C.



After solution treatment, the strength of GH2132 was significantly increased. Solid solution treatment can eliminate the precipitated phase in the alloy, reduce the number of grain boundaries and dislocations, and thus improve the strength of the alloy. The yield strength of GH2132 after solution is usually between 300 MPa and 500 MPa. GH2132 alloy has good deformation resistance under high temperature, high pressure and corrosion environment, and can withstand large forces without plastic failure. In addition, the toughness of GH2132 can be improved by solution treatment. Solution treatment can reduce the residual stress and grain boundary energy of the alloy, improve the toughness of the alloy, but also improve the ductility and impact toughness of the alloy, so that it has better heat resistance.

The elongation of GH2132 after solution is usually between 10% and 30%. This value can be adjusted according to the specific solution treatment conditions and heat treatment process. Elongation is a measure of the degree to which a material can undergo plastic deformation during stretching. The high elongation of GH2132 alloy after solution enables it to withstand stress in high temperature, high pressure and corrosive environment without plastic failure. GH2132 is widely used in aerospace, energy and chemical industries under high temperature, high pressure and corrosive environments.

评论